Company News

How to achieve UL94 V-0 rating for 1.5mm thick PC flame-retardant material?

2025-12-19 10:01:46
The following is a general conventional formula for PC modification, experimentally verified as an effective flame-retardant formulation. The addition amounts may vary slightly under actual working conditions; we welcome discussions and exchanges.
PC pellets + PC powder
  1. PC Flame Retardant
    YIMA SIFR-870M  0.5%
  2. PC Toughener
    KINGFOX USI-3310 1%
  3. PC Anti-Dripping Agent
    FLYHO K-PT205 0.4%
  4. Primary Antioxidant
    1010 0.1-0.15%
  5. Secondary Antioxidant
    168